  • **PU sealer, matt and glossy has to be mixed with the hardener in the ratio 80:20 of base and hardener. The mixture should be allowed to mature for at least 30 minutes and should be used within 4 hours of mixing.

  • ++Melamine sealer, matt and glossy has to be mixed with the hardener in the ratio of 90:10 of base and hardener. The mixture is to be allowed to mature for a minimum period of 30 minutes and should be used within 8 hours of mixing. Melamine should not be exposed to ammonia vapour at the time of mixing or application / drying.

  • ##Wood Stains gives the required shade to the wooden surface. Wood Stains can be mixed with Melamine, but not with TouchWood or PU wood sealer / finish. Wood Stains should be applied on raw wood before application of the clear coat or over the sealer coat, before the top coat. Wood Stains are for interior use only and will fade if applied on exterior wood. Normal Putty which is used to smoothen out walls cannot be used on wood. The previous coat of finish has to be very thoroughly sanded for the new finish adhesion.

Sr. No.

Name of Paint Thinner for 1 ltr/kg of paint in mls Thinner No. of coats recommended and application Undercoat applied Recoating Time (hrs)
1 Asian Paints Touch Wood Interior Brushing Spraying

0 - 50 or 200 -250

T -101 or MTO

1 to 2 Brushing or spraying

Wood filler if reqd.

12 - 16

2

Asian Paints Melamyne Sealer Brushing Spraying

200 - 300
200 - 300

T - 106 or T - 124

1 to 2 Brushing or spraying

Wood filler if reqd.

++8 - 10 
5 - 6

3

Asian Paints Melamyne Matt or Glossy Brushing Spraying

200 - 300
200 - 300

T - 106
T - 124

2 to 3 - Brushing or spraying

Wood filler followed by 1 coat Melamyne Sealer

++8 - 10
5 - 6

4

Asian Paints Melamyne Gold Clear Sealer Brushing Spraying

200 - 300
200 - 300

T - 106
T - 124

2 to 3 - Brushing or spraying

Wood filler followed by 1 coat Melamyne Sealer

++8 - 10
5 - 6

5

Asian Paints Melamyne Gold Clear Matt or Glossy Brushing Spraying

200 - 300
200 - 300

T - 106
T - 124

2 to 3 - Brushing or spraying

Wood filler followed by 1 coat Melamyne Gold Clear Sealer

++8 - 10
5 - 6

6

Asian Paints PU Sealer

150 - 300

PU thinner 338

2 to 3 - spraying only

--

**Min 12 and Max 72 between 2 coats

7

Asian Paints PU Interior and Exterior - Matt or Glossy

150 - 300

PU thinner 338

2 to 3 - By spraying only

PU sealer - Interior or Exterior sealer respectively.

**Min 12 and Max 72 between 2 coats

8

Asian Paints Touchwood Exterior Clear Glossy

Up to 50

T - 101 or MTO

3 - Coats By Brushing

No Wood Filler is applied

Overnight

9

Asian Paints Wood Stains##

--

NC Thinner or APCA NC Thinner 249

1 - 2 coats ragging except for Acrylic Wood filler it should be sprayed

Acrylic Wood filler or Melamyne or PU sealer

5 - 10 minutes between coats and 1 hr before finish coat

10

Asian Paints Acrylic Wood Filler

Up to 100 by wt.

NC Thinner or APCA NC Thinner 249

1 - 2 coats by putty applicator

--

3 hrs before Sealer or Finish coat